Wednesday, February 18, 2015

RE: [MW:22903] Weld Symbol Description

See below:

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nazrulla Khan
Sent: Wednesday, February 18, 2015 10:58 AM
To: materials-welding@googlegroups.com
Subject: [MW:22901] Weld Symbol Description

 

Gents,

Can any one explain the attached image weld symbol explanation.

1.      8 – depth of bevel
2.      7 – (5?) leg lengths of fillet weld
3.      2 – root opening of groove

4.     45deg – groove angle

 

Thanks & Regards

Nazrulla.JK

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPVF%2B2PUK7BF1zNpYvf_5bDKPS7F4z-iPVtem07Lj126t5CcsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...