Tuesday, October 21, 2014

Re: [MW:22158] WPS for Support

I think you may check and find suitable sWPS from ASME Sec. IX  and  submit it for approval to your client for only this job.


Regards


Tugrulhan OZDEMIR
QA/QC Welding Eng.

Saygılarımla / Regards


Tuğrulhan ÖZDEMİR

API 653 AI, Welding & Materials Eng.

Iraq mobile number: +964 782 311 67 81



2014-10-20 10:07 GMT+03:00 Richard robes <mech.processes@gmail.com>:
Dear ALL,

Please comment on the issue, Pipe to Shoe support fillet welding - Have WPS for SMAW process, can a welder do pipe to shoe support fillet welding in GTAW process.
Please note that for this specific project we don't have a wps qualified for GTAW process, only qualified wps for SMAW process.

Awaiting replies !

Regards
Richard

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...