Re: [MW:22153] ASME full form of SA - A 387/A 387M - 06a

“SA” is not an acronym.  It is just a designation given to the ferrous material specifications adopted by ASME to distinguish it from material specifications from other organizations.  There are also ASME “SB” specifications and they are for the nonferrous material specifications.  

 

The ASME SA- specifications are in ASME Section II, Part A and the ASME SB- specifications are in ASME Section II, Part B.  The latest edition is the 2013 edition.


On 17 October 2014 18:16, Anup N K E <nkeanup@gmail.com> wrote:

P91 stands for grade of the material , where P stands for pipe, 91 stands for 9% Cr, 1% Mo and Vanadium . P  no. Of grade P91 material is 15E.

Grade P9 has composition 9% Cr - 1% Mo whose P no. Is 5B.

Regards,
Anup N K E

On 17 Oct 2014 11:18, "Harish Kannepalli" <harishkannepalli@gmail.com> wrote:
American Society of Mechanical Engineers Section A, Developed by ASTM Commitee A01.11 A387/A387M is adopted from ASTM A387/387M where M stands for Metric; as Americans follow inch-pound system; 06 is year of publication, a-is first revision in that year
P91-P is desgination; 9%-Chromium, 1%Molybdenum

2014-10-17 10:40 GMT+04:00 Akhilesh singh <prof.akhileshsingh@gmail.com>:
Plz help me regarding such full-form:

1. ASME full form of SA - A 387/A 387M – 06a ............. what does means of "SA" - "A" 387 ................. "A387M" - "06a"..........................???

                          or
             A 387/A 387M – 06a

2. Grade P91 steel (A 387/A 387M – 06a)
    what does me "P"  & "91"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Mr. Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
With Regards
Binoy Lonappan

QAC Engineer





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...