Re: [MW:22123] SA 182 Gr. F11 Low Alloy Steel Welding - Preheat & Post heat Inquiry

what is pipe thicknees . if it is less than 16mm no pwht, but u have to do preheat, see ASME sec1 or B31.1

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY

On Thu, Oct 16, 2014 at 1:32 PM, Saravanan Sornam <saravanshyla@gmail.com> wrote:
Dear Welding Experts,

I need your advice to weld SA 182 Gr. F11, P No. 4 Gr. 1 as per ASME-IX,  Pipe to Cap Joint of 2 " , 8mm Thk., Single V Groove weld 

using SFA 5.28 , ER80S-B2 GTAW Filler, trade name T-80SB2, Kiswel, a Korean manufacturer.

1) As we do not have Client Spec for welding, I have checked in ASME- II C, Table-7, under
    Class ER80S-B2,  the Min. preheat is 135 Deg C and Max InterPass is 165 Deg C. this is 
    just a recommendation only right ? 

2) On the same table 7, under Notes C, it states, Prior to PWHT, can I follow the same
    statement in Notes C and send the material even after 1 day for PWHT after welding, 
    by proper post heat given in Notes C.
   
Because the PWHT location is quite far from our workshop.

) is there any chance of crack, if preheat comes below 135 Deg C, during welding ?

If you have any spec to weld this material, please share with me .

Regards,
Saravanan,
Korea

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...