How i can measure travelling speed and current in pulsed mode GTAW.
Because there are always 2 values of these parameters 1 for high pulse(HP) and  1 for low pulse(L).
i actually want to calculate heat input for this.so any guidance will be appreciated.
i.e. my data is
HP current 112 A
LP current 56 A
HP time 0.31 sec
LP time 0.31 sec
HP travelling speed 1 mm/min
LP travelling speed 150 mm/min
also can anyone tell me how can i find arc voltage value in machine data because i am using ORBIMAT 300 CA model of orbital welding machine and i can't find arc voltage value.thanx in advance
For more details i have attached a document with this Post.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...