Tuesday, October 28, 2014

[MW:22184] SUB: WPS HF OVERLAY WITH ITERMEDIATE LAYER OF 307Si

Dear Experts,

I have a typical problem. I request your expert guidance.

I have a requirement to do a HF overlay with stellite 6 on P1 base material using an intermediate (buffer) layer of SS 307Si.

My question is:

  1. In the WPS (per ASME SEC IX) do I need to do a separate PQR qualification test for intermediate layer as CR Overlay?
  2. Subsequently when I make HF overlay on the intermediate layer, which one is considered as base material (P1 material or intermediate metal)?
Thanks,
MANIVANNAN.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...