Tuesday, October 28, 2014

[MW:22182] Re: Underground Piping/Pipeline RT %

Hello

If your pipeline is in the scope of ASME B31.8 you should paragraph 826.2; other codes could have different requirements.



Sergio Antonio Muñoz Pinzón
IWE-IIW
http://Weld-ING.blogspot.com



El lunes, 27 de octubre de 2014 03:59:23 UTC-5, tugrulhan özdemir escribió:
Dear members


Is there anyone knows a code or standard mentioning the RT percentage for undergorund Piping or pipeline.




Regards



Tugrulhan OZDEMIR
API 653 Ins.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...