[MW:22134] ASME full form of SA - A 387/A 387M - 06a

Plz help me regarding such full-form:

1. ASME full form of SA - A 387/A 387M – 06a ............. what does means of "SA" - "A" 387 ................. "A387M" - "06a"..........................???

                          or
             A 387/A 387M – 06a

2. Grade P91 steel (A 387/A 387M – 06a)
    what does me "P"  & "91"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...