Re: [MW:15358] Normalise weld pass

0.5mm is allowed on the Basemetal adjacent to toe on the cap pass to avoid toe cracks and to meet Cap hardness requirements on HAZ>
 
Thanks & Regards

J.Gerald Jayakumar0091-9344954677
From: c.vijay kumar <vijay_online2003@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Friday, September 21, 2012 5:26 AM
Subject: [MW:15352] Normalise weld pass
Dear Experts,
 
Can you kindly clarify if the last weld pass is the normalise pass, then how much distance it should be from the edge of the groove. Is there any standard to give the distance in details.
why such a distance need to be maintained.
 
Regards,
Vijay
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm   The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.    

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...