Tuesday, July 31, 2012

Re: [MW:14994] Which Electrode/Filler wire we should use for 12Cr1MoV ?

Dear friend,

In 12Cr1MoV,the chromium content is only 0.9 to 1.2%. So we can use E8018-B2. In my 600MW chinese boiler all crown plates(Pr.parts support) are fabricated in 12Cr1MoV. Here we use only E8018 as per Chinese instruction.

Regards
Jubair

On Jul 31, 2012 9:58 AM, "Parveen Kumar Nakwal" <pknakwal@gmail.com> wrote:
Dear Experts,
 
In Thermal Power we have material of Strape plate is 15CrMo & we are using E8018B3,
 
Now New material 12Cr1MoV is coming for structure & piping work. Can we use ER 90SB3 + E9018 B3 ?which electrode & filler wire we should use as per standard.
 
If Not kindly suggest me Which Electore & filler wire should we use, as per the standards.
 
Waiting for Reply.
 
Regards.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...