Dear Expert
please advice-----
Recently we received some explosion bonded clad plate of SA516 gr 70 + SA 240 Tp 316L.
During explosion bonding plate having unbonded area.
As per SA 264 cl No 13.3.3 says that no single unbonded area exceeding 58cm2 with total unbonded area not to exceed 5% of the total cladded surface area.
Does it mean that above 58cm2 unbonded area are not acceptable or above 58cm2 unbonded area repairable upto 5% of total cladded surface area.
Thanks and Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...