Dear weld expert 

 
I have a one Question that is in welder test  P91 Material with welding process gtaw for root and smaw for fillup and caping.
Preheating also given 250 degree.  After cmplete the test pice can it is necessary do pwht  for welder qualification and Ndt process .

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.