Thursday, July 26, 2012
[MW:14963] F.No. for E309MoL
I need clear explanation As per ASME Sec IX, F.No. for E309MoL Electrodes in SFA 5.4.
It is confusing to clearly define the E309MoL Electrodes as F.No.4 or F.No.5.
So, please anyone can clarify.
Thanks & Regards
Gujula J Raju
QC Supervisor
GIWI SAUDI ARABIA LTD
SAMSUNG SAUDI ARAMCO PROJECT
Shaybah Inlet & Gas Treatment Project PKG#1
Shaybah, Kingdom of Saudi Arabia
Mob: +966 550858370
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...