[MW:14983] RE: 14980] Crosscountry Pipeline construction welding position of Pipe on hill

Dear sir,

If the pipe is inclined, it has to be 6G position.

Regards,

For Arc welding company,

Anil Verma

9999200148

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BHARAT GOLE
Sent: Monday, July 30, 2012 10:06 AM
To: Material Welding
Subject: [MW:14980] Crosscountry Pipeline construction welding position of Pipe on hill

 

In Crosscountry Pipeline construction what is welding position of Pipe on hill with respect to Welding Procedure as well as Welder qualification. Slope  of hill is around 30 °.

I had always  doubt whether it is  5G or 6G ? In fact I heard always debate on this issue.

Appreciate your expert comments soon.

Regards

Bharat B. Gole

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...