Dear Mr. Hiren,
 
As per Table 331.1.1 OF ASME B31.3, Max. Hardness 241 BHN.
 
B. R.
 
 
C. R. GANDHI

--- On Sat, 7/21/12, sevak hiren <hirensevak80@gmail.com> wrote:

From: sevak hiren <hirensevak80@gmail.com>
Subject: [MW:14916] welding & base metal hardness requirement for SA 387 Gr.5 Class II plate welding with E8018-B6
To: materials-welding@googlegroups.com
Date: Saturday, July 21, 2012, 11:27 AM

Dear Experts,
 
Can anyone provide welding & base metal hardness requirement for SA 387 Gr.5 Class II plate welding with E8018-B6.
 
Thanks & Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...