[MW:14909] RE: 14905] From GTAW bare filler with Ar shield to GTAW Fux Cored filler without Ar shield

You must requalify.  See essential variable QW-404.23  in the filler metal group in the list of variables for GTAW, QW-256.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal
Sent: Thursday, July 19, 2012 11:20 PM
To: materials-welding@googlegroups.com
Subject: [MW:14905] From GTAW bare filler with Ar shield to GTAW Fux Cored filler without Ar shield

 

Gents,
This one is related to switch over of GTAW electrode - from a bare one requiring Ar purging + shielding to the other flux cored one not requiring purging + shielding due to inaccessibility and large / long pipe sections under welding.
We have a WPS for using ER308L - Esab which requires Ar purging and shielding. But now, due to difficulties in maintaining Ar gas inside the long sections of large dia SS 304L pipes during root pass our contractor has suggested another electrode which does not need Ar purging + shielding.

Is this switch over allowed without re-qualification?

Alternate electrode suggested is this: KOBE TGX 308L STAINLESS STEEL FLUX CORED TIG WIRE (possibly 2.2 mm dia)

Thanks,

Shashank Vagal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...