Sir
On what basis is it not acceptable
Regards
Nitin
Sent from Nitin Shetty iPhone
On Jul 18, 2012, at 6:01 AM, Swapnil Vanjara <swapnil.vanjara@gmail.com> wrote:
> not acceptable
>
>
> On 7/14/12, sevak hiren <hirensevak80@gmail.com> wrote:
>> At the time of forming the spin hole dia was less than 60 mm around 30 mm,
>> but while forming the crack was observed at spin hole, so the hole was
>> extended to 70 mm & the patch was welded. RT is also done for patch weld.
>>
>> But as per Section VIII Div I, is it acceptable ?
>>
>> On Fri, Jul 13, 2012 at 5:01 PM, Swapnil Vanjara
>> <swapnil.vanjara@gmail.com>wrote:
>>
>>> first of all tell me haw ur dia bcm more than 60
>>>
>>>
>>> On 7/13/12, Swapnil Vanjara <swapnil.vanjara@gmail.com> wrote:
>>>> first of all tell me haw ur dia bcm more than 60
>>>>
>>>>
>>>> On 7/13/12, sevak hiren <hirensevak80@gmail.com> wrote:
>>>>> Dear Experts,
>>>>>
>>>>> As per ASME section VIII Div I , UW-34, max. allowable patch diameter
>>> for
>>>>> a
>>>>> spin hole of dishend is 60 mm.
>>>>>
>>>>> If, the dish end spin hole patch diameter is found to be of more than
>>>>> 60
>>>>> mm
>>>>> then the dish end should be rejected, please correct me if I am wrong.
>>>>>
>>>>>
>>>>> Thanks in advance.................
>>>>>
>>>>> --
>>>>> To post to this group, send email to
>>>>> materials-welding@googlegroups.com
>>>>> To unsubscribe from this group, send email to
>>>>> materials-welding+unsubscribe@googlegroups.com
>>>>> For more options, visit this group's bolg at
>>>>> http://materials-welding.blogspot.com/
>>>>> The views expressed/exchnaged in this group are members personel views
>>>>> and
>>>>> meant for educational purposes only, Users must take their own
>>>>> decisions
>>>>> w.r.t. applicable code/standard/contract documents.
>>>>>
>>>>
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>> The views expressed/exchnaged in this group are members personel views
>>> and
>>> meant for educational purposes only, Users must take their own decisions
>>> w.r.t. applicable code/standard/contract documents.
>>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment