Hi Gents
Be aware that this Code requirement is only applicable if the cladding is
taken into consideration for the strength of the vessel. If it is only
applied for corrosion resistance, this Code requirement is not applicable.
The max. size of the unbonded area is than only limited to locations of
openings or tubeholes (in case of a tubesheet)
Regards
Fred Bosman
-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens krishna mudhale
Verzonden: maandag 23 juli 2012 14:38
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:14936] Repair of cladding plate as per SA 264
But question is that when the repair area has to be repaired either
area exceeds 58cm2 or less.
On 7/23/12, Vinayak Kale <Vinayak_Kale@lntenc.com> wrote:
> It means , unbounded area to be removed & repair , recently i have face
the
> same problem in cladded dish end , we removed complete cladded area by
> machining & rewelded with SAW process
>
> Regards
>
>
> Vinayak Kale
> OGSP - QA & I , HC - Upstream
> EPC Block , 2nd Floor , Gate No.1
> Saki Vihar Rd. Powai Campus
> Mumbai - 400072
> Ph : + 91 022 6705 3969
> (M) - 9987875309
> www.larsen toubro.com
>
>
> -----materials-welding@googlegroups.com wrote: -----
>>
>> To: materials-welding@googlegroups.com
>> From: kundan.ahirao@gmail.com
>> Sent by: materials-welding@googlegroups.com
>> Date: 07/23/2012 12:23PM
>> Subject: [MW:14925] Repair of cladding plate as per SA 264
>>
>> Dear Expert
>> please advice-----
>> Recently we received some explosion bonded clad plate of SA516 gr 70 + SA
>> 240 Tp 316L.
>> During explosion bonding plate having unbonded area.
>> As per SA 264 cl No 13.3.3 says that no single unbonded area exceeding
>> 58cm2 with total unbonded area not to exceed 5% of the total cladded
>> surface area.
>> Does it mean that above 58cm2 unbonded area are not acceptable or above
>> 58cm2 unbonded area repairable upto 5% of total cladded surface area.
>>
>> Thanks and Regards
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views
and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment