Re: [MW:14986] RE: 14980] Crosscountry Pipeline construction welding position of Pipe on hill

 Mr. Bharat,

 For hill locks/slopes, it should be 6G - (pipe inclined to 45deg -welding in vertical
 down) using  E6010 (or) any E xxx0 for root  application, followed by E7013 (or) any    
 E xxx3 for hot pass.

 It covers  both 6G and 5G position used in plain terrains (pipe - horizontal) also.

 sridhar.


From: ARC WELDING COMPANY <arcweldingcom@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 30 July 2012 12:58 PM
Subject: [MW:14983] RE: 14980] Crosscountry Pipeline construction welding position of Pipe on hill

Dear sir,
If the pipe is inclined, it has to be 6G position.
Regards,
For Arc welding company,
Anil Verma
9999200148
 
 
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BHARAT GOLE
Sent: Monday, July 30, 2012 10:06 AM
To: Material Welding
Subject: [MW:14980] Crosscountry Pipeline construction welding position of Pipe on hill
 
In Crosscountry Pipeline construction what is welding position of Pipe on hill with respect to Welding Procedure as well as Welder qualification. Slope  of hill is around 30 °.
I had always  doubt whether it is  5G or 6G ? In fact I heard always debate on this issue.
Appreciate your expert comments soon.
Regards
Bharat B. Gole
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...