What is your soaking temperature? If it is higher than 1100F, then you can adjust your time by measuring the time it reaches 1100F on the heating and cooling rate and thereby making your time longer, by about 5 minutes? IF not, then you have to send it back for another 5 minutes in the over, which is really...
 
 
 


 
On Sat, Jul 21, 2012 at 12:52 AM, mohd <mohd52100@gmail.com> wrote:
Dear expert,

As per ASME 8-1-UCS-56

We have done SR for our 40mm thk-30" pipe joint.

but unfortunetly, soaking time was just short by 5min.Now our client/PMC both are not agree to release.

Required time : 1hr.15min
Actual Time : 1hr.10min

It is acceptable OR could you share any technical view to convince client?

regards,
mohd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...