[MW:14987] RE: 14980] Crosscountry Pipeline construction welding position of Pipe on hill

Dear All,

 

This position is 100%- 6G only no need to doubt in this matter – (for clarification may refer to Sec IX)

 

And 5G will come for the pipe on the ground position – not involved any angular position.

 

Thanks and Regards................?

 

Lakshman Kumar.B|Manager |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of BHARAT GOLE
Sent: Monday, July 30, 2012 10:06 AM
To: Material Welding
Subject: [MW:14980] Crosscountry Pipeline construction welding position of Pipe on hill

 

In Crosscountry Pipeline construction what is welding position of Pipe on hill with respect to Welding Procedure as well as Welder qualification. Slope  of hill is around 30 °.

I had always  doubt whether it is  5G or 6G ? In fact I heard always debate on this issue.

Appreciate your expert comments soon.

Regards

Bharat B. Gole

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...