It means , unbounded area to be removed & repair , recently i have face the same problem in cladded dish end , we removed complete cladded area by machining & rewelded with SAW process  

Regards


Vinayak Kale
OGSP - QA & I , HC - Upstream
EPC Block , 2nd Floor , Gate No.1
Saki Vihar Rd. Powai Campus
Mumbai - 400072
Ph : + 91 022 6705 3969
(M) - 9987875309
www.larsen toubro.com


-----materials-welding@googlegroups.com wrote: -----
To: materials-welding@googlegroups.com
From: kundan.ahirao@gmail.com
Sent by: materials-welding@googlegroups.com
Date: 07/23/2012 12:23PM
Subject: [MW:14925] Repair of cladding plate as per SA 264

Dear Expert
please advice-----
Recently we received some explosion bonded clad plate of SA516 gr 70 + SA 240 Tp 316L.
During explosion bonding plate having unbonded area.
As per SA 264 cl No 13.3.3 says that no single unbonded area exceeding 58cm2 with total unbonded area not to exceed 5% of the total cladded surface area.
Does it mean that above 58cm2 unbonded area are not acceptable or above 58cm2 unbonded area repairable upto 5% of total cladded surface area.

Thanks and Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...