Re: [MW:14969] SS Electrode Eccentricity Tester

Mr. Ahmad,

The electrode  coating (eccentric)  testing is ment for all types of electrodes
including SS also.

We have used the tester for all types of electrodes in the plant.

sridhar.

From: Ahmad Ghauri <murtaza506@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Friday, 27 July 2012 4:01 PM
Subject: [MW:14968] SS Electrode Eccentricity Tester

Dear All

We have an eccentricity tester that determines the eccentricity of SMAW electrodes containing MS core wire.
Is there any tester that determines the eccentricity of SMAW electrodes containing SS core wire???


Regards,
AHMAD
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...