Dear Maganth,
 
I assume person from the TPI is good in technical.
 
Assume the product may be in the Jack case applications in Shipbuilding or similar applications.
 
In order to reduce the fabrication time , they will go for the forged rather than the 2 pcs then weld again.
 
In that cases, the best way to do welding simulation by welding the actual test pcs by approved WPS.
 
Majority of the cases, the forged company will supply small test pcs from the production heat for the verification to the customer approval
 
If the plate thickness is more than 100 mm , it is suggested to do verification of WPS in actual forged steel materials
 
Since the forged materials , may be less in CVN and elongation , it is better to verify the mechanical properties in the actual pcs after welding by approved WPS.
 

 
On Wed, May 30, 2012 at 1:00 PM, Lab <lab@cochinshipyard.com> wrote:
Dear Friends,
 
In our production unit, we would like to make butt weld between forged steel grade of S355J2G3, a round shaped object. The Third part Inspection (TPI) agency which clears the joint, insists us to perform WPS on similar material before production welding. This particular material was imported from other country long back and we could not thick about WPS when we purchased. It is not possible for us to get the similar material (same grade & same condition) suitable for WPS as well as WPQ and no response from the suppliers when contacted for supply of small quantity.
 
At last one supplier came forward and ready to supply S355J2G3 of rolled and normalized plate.
 
When we went to TPI with the proposal of making WPS with rolled plate, they are not convinced as the properties of forged and rolled steel even after Normalizing, are different and insisting us to do WPS test on forged steel of same grade.
 
Request the forum to provide guidelines to get rid of this situation or from where I get small quantity of material of similar grade, condition in India to arrange for WPS.
 
Regards,
Megnath
The information contained in this message are Cochin Shipyard Limited confidential and proprietary information and is intended only for the use of the recipient(s) named above. If the reader of this message is not the intended recipient, he/she is hereby notified that any use, dissemination, distribution, or copying of this communication or any of the content is strictly prohibited. In such case, please advise the sender immediately and delete it from your system. Further acknowledges that any views expressed in the message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Cochin Shipyard Limited.      ----------------------------------  Cochin Shipyard Ltd, Cochin, India      !-- Virus-Free Mail Using AntiVirus for PostMaster Enterprise & QuickHeal Engine --!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...