Monday, May 28, 2012

Re: [MW:14377] castable refractories

Sir,
Enclosed Met-Chem lab(Vadodara) details may serve your purpose.
 
In addition to that RK laboratory(Delhi) also having the Cast able refractory testing up to 1200 deg.C.
Regards,
 
Venkat..
On Sat, May 26, 2012 at 4:29 PM, K.M Hrishikesan <hrishikm07@gmail.com> wrote:
Hi
 
Can somebody suggest few testing laboratories in India where I can test castable refractories as per IS:10570
 
Thanks
 
Hrishi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

With Regards,

 

VENKATA BALARAM.INTI | Assistant Manager - QA/QC|

HPCL-Mittal Energy Ltd| Guru Gobind Singh Refinery - Project.|

Phullokhari - Bathinda (PB.) - 151301.| Telefax: 01655 - 241775, Off: 01655 272466

+91-9988885390 |E mailto:venkata.inti@hmel.in

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...