[MW:14344] ASTM A516Gr.70 Plate is not accepted for LPG Bullet fabrication as well as Low Temperature service equipment & Piping.


Dear All,
At the time of LPG Bullet of fabrication unavailability of ASTM A516 Gr.60 at Indian Market our contractor used at the position of Bullet nozzle self reinforcement plate thickness of 75mm  ASTM A516Gr.70 in place of ASTM A516Gr.60.
According to OISD standard 144(Second Edn., 2005), for LPG installations clause 6.2.1 point(ii):- Material shall be in line with design code. ASTM A516 Gr.60 shall be used for refinery service and for marketing installation where H2S is not present ASTM A516 Gr.70 or A537 CLASS 1 can be used. Micro-alloyed stell containing NI.Mo,Va shall not be considered. Maximum specified tensile stress shall not be more than 80,000psi.
As per MTC Manganese ./.age is 1.37, however as per code it should be 0.85 - 1.20.
So pleased clarified me why ASTM A516 Gr.70 material is not accepted as per metallurgy as well as service point of view.
And also Advised me what based we can accepted of ASTM A516 Gr.70 material in placed of ASTM A516 Gr.60 as per metallurgy as well as service point of view, if any testing is required for acceptance the said material.
--
Thanks & Regards
Pinaki Boxi.

Mob-+919178466059


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...