[MW:14343] 70-30 Cu, Ni tube pitting

Dear friends,

We are having surface condenser where steam is condensing by using sea water. sea water in tube side and condensate in shell side under vacuum. It has been failed due to tube leaking and tube failure due to pitting it is not due to erosion. it is also strange that pitting not only in the tube ID sea water side but also in the OD. 

So please Advice what may be the reason.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...