Hi, Can any one tell whether I can carry out PWHT of clean out door
welding after erection of first shell course?
We have erected the clean out door section of the shell plate and
completed vertical welding without performing the PWHT. As per API
650, it needs to be completed PWHT regardless of thickness before
assembly(erection).
if that is the case, I have to cut the joint and do the PWHT and
reweld again.Can I do PWHT at site after erection?
If not, any one explain me what is the reason behind it. Why API is
insisting to have PWHT before erection.
Cheers,
Thomas
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment