Dear friend,
B31.3 there have given teh acceptance for the root concavity
check table:341.3.2
check the density of the root and parrent material.. its should
not more than parent materialn at concavity side ( lenght is not given
we dont want to considered )
API 510 we have accpetance its should not be more 6mm lengh of concavity
depth same
Regards
sankar.k
On 5/30/12, Vu Duc Thuan <dthuan117@gmail.com> wrote:
> Dear Expert,
>
>
>
> In my project, we have some tubing line ( ½" SS316L and Duplex) need to
> weld
> with reducer same material, we have WPS for both of material. The problem
> is
> the RT report show internal concavity but we do not have accept criteria
> for
> those weld joints as per drawing, Spec..etc..
>
>
>
> Kindly please advise which code & standard are using for the tubing. (
> tubing fix on the hydraulic control panel )
>
>
>
>
>
> Regards,
>
>
>
> Thuan
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
shankar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35668] Selection of Filler/Electrode.
Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment