Re: [MW:14394] Welding Electrode for galvenised Iron(GI)

Weld with a rutile flux electrode, the rutile will help minimize the
potential fro cracking caused by the Zinc.

To repair the galvanizing after welding use a Galvanizing Repair Rod
http://www.zaclon.com/pdf/alloy_repair_rods_data.pdf.

Richard


Original Message:
-----------------
From: Roy Liu standardliu@hotmail.com
Date: Tue, 29 May 2012 19:35:58 +0800
To: materials-welding@googlegroups.com
Subject: Re: [MW:14389] Welding Electrode for galvenised Iron(GI)


Brazing is the best way to weld such kind of material. otherwise the
Galvansied layer will be destroied.

Roy
Bohler Welding Group

From: shashi pandey
Sent: Monday, May 28, 2012 11:37 PM
To: materials-welding@googlegroups.com
Subject: [MW:14385] Welding Electrode for galvenised Iron(GI)


Dear Experts,
Can you please suggest me about best welding electrode for galvenised
Iron(GI) pipe/plate etc.?
What will be the effect on GI materials if it will be welded with MS/CS
welding electrode?
--


With Thanks....?

SHASHI B. PANDEY |SR. ENGINEER(MECHANICAL) |LANCO GROUP.

RAJNANDGAON, CHHATISHGARH | MOBILE: +91 8305357495

| Go Green | The future will thank you |

--------------------------------------



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.


--------------------------------------------------------------------
mail2web.com – What can On Demand Business Solutions do for you?
http://link.mail2web.com/Business/SharePoint


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...