Re: [MW:14350] Sample test or tubular mock-up test for 6GR

Dear Mr.Park,
 
Please refer and follow AWS D1.1 Table-4.1 and Table 4.5 for Essential Varaiables for Welding Position.
 
For testting, you can refer clause 4.12 for tubular connections.
 
Hope U can search all these from Section 4, AWS D1.1.
 
FYI, I am working for KC Cottrell, Anseong city, Gyeonggi-do Korea.
 
Cheers,
SARAV.
Anseong, Korea
010-7218-1706
 
 

On Thu, May 24, 2012 at 7:16 AM, 박종민(PARK, JONG MIN) <carpediem@dsme.co.kr> wrote:

Dear Experts

 

WPS for 6GR could be developed via 6GR coupon in accordance with AWS D1.1.

However, sample test or tubular mock-up test is required from time to time.

 

1st question

 Are they mandatory for all 6GR qualification test?

2nd question

Can fabricator select test method, sample test or tubular mock-up ?

 

Your prompt advice would be highly appreciated.

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...