Dear all,
Use Stainless steel E308L electrode from
AVESTA Brand were u can avoid such kind
of problem. Red hot condition. is mainly
due to non uniformity of flux coat
Neilashkumar
Welding Engineer
NOV
------------------------------
On Tue 29 May, 2012 5:33 PM IST murtaza506@yahoo.com wrote:
> I have a MMA welding electrode of SS 308L Dia. 2.6mm. when half of
>the electrode is consumed it get red hot, and it gives porosity in the
>weld metal what could be the reason i.e. is it a welding problem or
>there is a problem in the electrode???
>if this problem is due to electrode then what can be the reasons and
>rectifications???
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment