You can use Carbon Steels with Nace Quality ( Controlled Composition of Alloys).
Ex SA 516 60 ( Nace for Sulphide Cracking)
Some of the clients want Heat Treatment after fabrication.
Aniket Gupta
On 5/20/12, vnbhatt@gmail.com <vnbhatt@gmail.com> wrote:
> Respected Material Experts,
>
> We have a pharmaceutical client inquiry where they have gas media with 60 %
> H2S gas in the mix with 500 PPM moisture flowing from piping, vessels and
> shell-tube exchanger under pressure of 37 bar gauge.
>
> With many experienced brain on group, I seek details as to what MOC to be
> employed, what quality checks and what corrosion allowance??
>
> Appreciate guidance.
>
> Regards,
>
> Vinod Bhatt
> Sent on my BlackBerry® from Vodafone
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Ex SA 516 60 ( Nace for Sulphide Cracking)
Some of the clients want Heat Treatment after fabrication.
Aniket Gupta
On 5/20/12, vnbhatt@gmail.com <vnbhatt@gmail.com> wrote:
> Respected Material Experts,
>
> We have a pharmaceutical client inquiry where they have gas media with 60 %
> H2S gas in the mix with 500 PPM moisture flowing from piping, vessels and
> shell-tube exchanger under pressure of 37 bar gauge.
>
> With many experienced brain on group, I seek details as to what MOC to be
> employed, what quality checks and what corrosion allowance??
>
> Appreciate guidance.
>
> Regards,
>
> Vinod Bhatt
> Sent on my BlackBerry® from Vodafone
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments