Dear Mr.Hrishi,
You can go for the following companies for the castables as per BIS 10570-:
A) Calderys India Refractories,Katni (M.P.)
B) Castwel Industries,Nagpur(Maharastra)
C) S.K.G.Refractories,Butibori,Nagpur(Mahrastra)
D) Abs Refractories,Niwar(M.P.)
The mentioned companies are manufactures of castables & bricks which
are doing testing also on commercial basis.
More details you can get on internet.
Thanks,
S.D.Mishra(Sr.Inspection Engineer)
On 5/26/12, K.M Hrishikesan <hrishikm07@gmail.com> wrote:
> Hi
>
> Can somebody suggest few testing laboratories in India where I can test
> castable refractories as per IS:10570
>
> Thanks
>
> Hrishi
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
Thanks,
S.D.Mishra
Mob- +91-9981237879 (M.P./C.G.)
+91-9766916581 (Maharastra)
Reach for the moon, even if you miss you'll land among the stars!!!!!!!
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment