Monday, May 28, 2012

[MW:14382] Hardfacing overlay on SA 572 GR 50 PLATE by IRON BASE RODS

Dear All,
 
Greetings.
 
A hardfacing overlay has to be carried out on  A572 GR 50 Plate by FCAW - Semiautomatic Process as per ASME SEC IX.
 
rod used will be iron based.
 
please inform me what will be the SFA No. how we can decide A No.
 
Please give code reference.
 
Thanks & Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...