Tuesday, May 1, 2012

Re: [MW:14169] welding SS316L to Super Duplex SS

As per ASME SEC IIC they are recommending ENiCrFe-12 electrode. But if service temprature is below 350 C you can go for E309LMo.

Best Regards,

Sandeep Singh

Welding Engineer

Essar Heavy Engg Services.


From: Himan Nikdin <himannikdin@gmail.com>
To: materials-welding Group <materials-welding@googlegroups.com>
Sent: Sunday, April 29, 2012 4:20 PM
Subject: [MW:14161] welding SS316L to Super Duplex SS

Dear Experts

Would you please suggest me a welding consumable for welding SS316L (pipe) and Super Duplex (UNS 32750) (pipe), the joint is for pipe support and not in service.

regards,
Himan
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.