Dear Expert,

 

Please advise me (clear my doubt) if my 6G Welder can carry-out the work with the following info . My welder qualification is at 3.5” (OD)[WT=12.7mm]. While the actual work is 4”OD [WT=8.56 mm(Sch 80)].

 

I will allow my welder to carry-out welding with the concession of monitoring his progress by NDT-RT. How often do I take RT? (is it 10% of his weld joint as per BS and ASME std?) Please revert and advise. Thank you!

 

 

Respectfully yours,

Peter Paul

 

+65 9939 5904

 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...