Thursday, April 5, 2012

Re: [MW:14065] defects in Radiographic interpretetion - an illustration

Dear expert,
 
Good afternoon,
 
Any one suggest how to distinguish between root under under cut(RUC) and elongated slag inclusion  during  RT interpretation.
 
Thanks
SAJID

On Thu, Apr 5, 2012 at 10:40 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:

http://www.4shared.com/office/BwNoWtwO/Welding_Errors_.html


---------- Forwarded message ----------
From: Harry Patel <harryeng...@gmail.com>
Date: Nov 2 2011, 4:39 pm
Subject: Welding Defect Photo
To: Materials & Welding


Dear Sirs,

Anybody have welding defect photo like incomplet fusion,incomplete
penetration, root concavity in pipe.

I hope for your reply.

Thank you very much in advance.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.