Re: [MW:14155] radiography for roof manhole nozzle.

manhole roof nozzle weld may not permit acceptable RT due to the joint configuration, due to shadow by nozzle on film or artefacts from partial film contact on area of intrest. otherwise UT for class 1 test or optional MT for class 2 test reqmts.
------------------------------
On Tue, Apr 24, 2012 9:39 AM EDT SACHIN wrote:

>Dear experts plz advice is it mandatory to take radiography for roof
>manhole mozzle as per api 650
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...