As per API 650

2.2.1.4

Shell plates are limited to a maximum thickness of

45 mm (1.75 in.) unless a lesser thickness is stated in this

standard or in the plate specification. Plates used as inserts or

flanges may be thicker than 45 mm (1.75 in.). Plates thicker

than 40 mm (1.5 in.) shall be normalized or quench tempered,

killed, made to fine-grain practice, and impact tested.

Regards,
 
J.N.Murthy
 
On Fri, Apr 20, 2012 at 8:59 PM, manoj john <manojacgnr@gmail.com> wrote:
Dear All,

Can anyone give information for the impact test requirement as per API 650 for carbon steel plate thickness for atmospheric storage tank.

Thanks & Regards.
Manoj 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...