[MW:14161] welding SS316L to Super Duplex SS

Dear Experts

Would you please suggest me a welding consumable for welding SS316L (pipe) and Super Duplex (UNS 32750) (pipe), the joint is for pipe support and not in service.

regards,
Himan

--