Wednesday, April 11, 2012

Re: [MW:14092] Welding Grey Cast Iron (Repair)

Dear Expert,
 
U can try with Xuper 2240 of L&T
 
= s p raman=
 
----- Original Message -----
Sent: Monday, April 09, 2012 4:47 PM
Subject: [MW:14084] Welding Grey Cast Iron (Repair)

Hi,

 

Can anybody provide me with any reference article for welding Grey Cast Irons?

 

Thanking you,

Rgds,

 

Prashant

 

 

 

 

 

 



Any views or opinions expressed in this email and its attachments are those of the individual sender except where the sender specifically states them to be that of Lamprell.

This E-mail and any attachments are confidential and may also be legally privileged. If you have received this email and any attachments in error, you are on notice of its status. Please (a) notify the sender immediately by reply email; (b) destroy this email and any attachment, and (c) do not use, copy, store and/or disclose to any person this email and any attachments: to do so could be a breach of confidence. Thank you for your co operation. Please contact the Lamprell IT Helpdesk on ithelpdesk@lamprell.com if you need any assistance.

Holding company: Lamprell plc, incorporated in the Isle of Man, registration number 117101C, registered office at Fort Anne, Douglas, Isle of Man IM1 5PD

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...