RE: [MW:14107] Re: Regarding Electrode Weaving

Also in addition to the Maulik’s reply, please take a note that more is the weaving width in that particular area which implies more heat input for that area due to low travel speed, lesser weld metal deposit (that depends on your travel speed) and slower is the cooling rate  which results in the grain coarsening in that area. When impact is taken from that part of the weld, there are more chances to getting it to a failure.

 

Hence we restrict it.

 

Thanking you,

Rgds,

Prashant

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Maulik Thakkar
Sent: Thursday, April 12, 2012 6:42 PM
To: Materials & Welding
Subject: Fwd: [MW:14105] Re: Regarding Electrode Weaving

 

As your weaving width increases there will be maximum chances of slag entrapment at both sides (left & right) because of prior solidification of weld before welding of respective edges. Your weld pool should be in fused state during weaving to avoid slag entrapment.

Regards,
Maulik
Welding Engineer
Larsen & Toubro

---------- Forwarded message ----------
From: Karthik <karthik6684@yahoo.com>
Date: Wed, Apr 11, 2012 at 9:38 AM
Subject: [MW:14091] Re: Regarding Electrode Weaving
To: Mohit Aggarwal <aggarwalmohit05@gmail.com>, "george.dilintas@gr.bureauveritas.com" <george.dilintas@gr.bureauveritas.com>, AA karandish <aa.karandish@yahoo.com>, Abuhanip bin Abdul <abuhanip@labuanship.com>, Ahmed Osman <a.osman81@yahoo.ca>, akcme <akhilcme@gmail.com>, Ali Asghari <asghariali@rocketmail.com>, Aly <mhaskar.aly@gmail.com>, AMIT PAHUJA <amitpahuja2@gmail.com>, Amos Majola <amos@turnmill.co.za>, Anil Hegde <nottyanil@gmail.com>, antony jenis <antonyjenis@gmail.com>, Arun Jacob <jacob.igcs@gmail.com>, Arunachalam A <arunvani@gmail.com>, Ary Agung Prasetyo <ary_mt05@yahoo.com>, asad azmi <azmiasadayub@gmail.com>, Brl Pp <refazosaris@gmail.com>, Dindo <dindodelacruz@gmail.com>, Dinesh Somwanshi <som.din@gmail.com>, duc hoang <hoangvanduc79@gmail.com>, ENAYAT ZAREI <zarei.enayat@gmail.com>, Endri Prasetyo <endri.prasetyo@gmail.com>, Fitria Rahman <t.chintaqa@gmail.com>, fredric <fredric.prabu@bwgindia.com>, "Garry Mat Eng." <garryirwin342@gmail.com>, Himan Nikdin <himannikdin@gmail.com>, james gerald <gerry_tup@yahoo.com>, John Henning <jhenning@deltak.com>, jose <joseseban@gmail.com>, Kaja Mohideen <kaja@asw.sa>, kannayeram gnanapandithan <kgpandithan@gmail.com>, Kavin Murugam <kavin202082@yahoo.com>, ketan shah <ai.ketan@gmail.com>, khemici badri <khemicib@yahoo.fr>, lakshman kumar <lakshmankumar4@gmail.com>, Madhusudan Rout <madhusudan.rout@gmail.com>, mahesh sanghvi <sls.mahesh@gmail.com>, Mahmoud <mqreis@gmail.com>, materials-welding <materials-welding@googlegroups.com>, meemo prasad <meemoprasad@gmail.com>, Mehdi Emami <mehdi.emami@yahoo.com>, mpk mpk <ranmi2007@gmail.com>, MRG <mrgupta_2007@yahoo.com>, muthu barathi <muthu_barathi@rediffmail.com>, "Nadgauda, Subhas" <subhas.nadgauda@jacobs.com>, Nandesh Kumar <nandeshkumar@rocketmail.com>, Narendra Gohil <ngohil@qafco.com.qa>, Neilash Kumar <neilashkumar@yahoo.com>, Nizam Mohamad <ahmad.nizam83@yahoo.com>, pgoswami <pgoswami@quickclic.net>, Pieper QSI <info@pieper-qsi.nl>, "prabhakarmet@gmail.com" <prabhakarmet@gmail.com>, prem nautiyal <prem_nautiyal26@yahoo.com>, "R.Lenin" <lenin8319@gmail.com>, rajeev arora <rajeevarora007@gmail.com>, rajkumarantoni <antonitr@gmail.com>, Ramchandra vichare <vicharerke@indiatimes.com>, Ramin Kondori <raminkondori@gmail.com>, ravi varman <ravimvarman@gmail.com>, S C Balawat <scb12345@gmail.com>, sanggyu LEE <sgleehong@gmail.com>, santhosh kumar <santhoshgu7@gmail.com>, SAQIB SHIRAZI <saqibshirazi83@hotmail.com>, sevak hiren <hirensevak80@gmail.com>, shanmuga mari <85.ssmari@gmail.com>, snbagchi <snbagchi@aol.in>, Srinivas Engr <srinivas.gmsrini@gmail.com>, srinivasu <srinivasu.mech@gmail.com>, "T. Mahendran" <cbemahendar@yahoo.com>, U WYNN-NAING <u.wynn-naing@total.com>, vaibhav Joshi <vnjoshi.leo@gmail.com>, venkat ramana <venkatgps.ramana@gmail.com>, Vijay Katkar <katkar.vijay22@gmail.com>, "vinit.deshpande" <vinit.deshpande@akersolutions.com>, Vino Varghese <vinopvarghese@gmail.com>, Wu Hua <jointstars@yahoo.com>, yogeshkumar Kumbhar <kumbharyogeshv@gmail.com>, ZUL MAS <zulmas77@yahoo.com>

Hi,

As per Code it is a Non essential variable and Code doesn't specify the weave bead width limits. But you have to specify on the WPS (Stringe/Weave bead). Its a good engineering practice to limit the weave bead width to control the heat input.

 

Thanks & Regards,

 

(Karthik)

 

Karthikeyan.S

QA/QC Manager

German-Thai Boiler Engineering Cooperation Limited.

Rayong Factory ;

379 Moo.6 Soi 8, Tambol Pananikom,

Nikompattana, Rayong 21180 THAILAND

Tel : +66 38 897 035-9 Ext. 137

Fax : +66 38 897 034

Hand Phone: 0066 892512282

 

From: Mohit Aggarwal <aggarwalmohit05@gmail.com>
To: christopher_rajku...@yahoo.com; george.dilintas@gr.bureauveritas.com; manojac...@gmail.com; welding_engr_r...@charter.net; AA karandish <aa.karandish@yahoo.com>; Abuhanip bin Abdul <abuhanip@labuanship.com>; Ahmed Osman <a.osman81@yahoo.ca>; akcme <akhilcme@gmail.com>; Ali Asghari <asghariali@rocketmail.com>; Aly <mhaskar.aly@gmail.com>; AMIT PAHUJA <amitpahuja2@gmail.com>; Amos Majola <amos@turnmill.co.za>; Anil Hegde <nottyanil@gmail.com>; antony jenis <antonyjenis@gmail.com>; Arun Jacob <jacob.igcs@gmail.com>; Arunachalam A <arunvani@gmail.com>; Ary Agung Prasetyo <ary_mt05@yahoo.com>; asad azmi <azmiasadayub@gmail.com>; Brl Pp <refazosaris@gmail.com>; Dindo <dindodelacruz@gmail.com>; Dinesh Somwanshi <som.din@gmail.com>; duc hoang <hoangvanduc79@gmail.com>; ENAYAT ZAREI <zarei.enayat@gmail.com>; Endri Prasetyo <endri.prasetyo@gmail.com>; Fitria Rahman <t.chintaqa@gmail.com>; fredric <fredric.prabu@bwgindia.com>; Garry Mat Eng. <garryirwin342@gmail.com>; Himan Nikdin <himannikdin@gmail.com>; james gerald <gerry_tup@yahoo.com>; John Henning <jhenning@deltak.com>; jose <joseseban@gmail.com>; Kaja Mohideen <kaja@asw.sa>; kannayeram gnanapandithan <kgpandithan@gmail.com>; Karthik <karthik6684@yahoo.com>; Kavin Murugam <kavin202082@yahoo.com>; ketan shah <ai.ketan@gmail.com>; khemici badri <khemicib@yahoo.fr>; lakshman kumar <lakshmankumar4@gmail.com>; Madhusudan Rout <madhusudan.rout@gmail.com>; mahesh sanghvi <sls.mahesh@gmail.com>; Mahmoud <mqreis@gmail.com>; materials-welding <materials-welding@googlegroups.com>; meemo prasad <meemoprasad@gmail.com>; Mehdi Emami <mehdi.emami@yahoo.com>; mpk mpk <ranmi2007@gmail.com>; MRG <mrgupta_2007@yahoo.com>; Muhammed Ibrahim PK <ibrat...@gmail.com>; muthu barathi <muthu_barathi@rediffmail.com>; "Nadgauda, Subhas" <subhas.nadgauda@jacobs.com>; Nandesh Kumar <nandeshkumar@rocketmail.com>; Narendra Gohil <ngohil@qafco.com.qa>; Neilash Kumar <neilashkumar@yahoo.com>; Nizam Mohamad <ahmad.nizam83@yahoo.com>; pgoswami <pgoswami@quickclic.net>; Pieper QSI <info@pieper-qsi.nl>; "prabhakarmet@gmail.com" <prabhakarmet@gmail.com>; prem nautiyal <prem_nautiyal26@yahoo.com>; R.Lenin <lenin8319@gmail.com>; rajeev arora <rajeevarora007@gmail.com>; rajkumarantoni <antonitr@gmail.com>; Ramchandra vichare <vicharerke@indiatimes.com>; Ramin Kondori <raminkondori@gmail.com>; ravi varman <ravimvarman@gmail.com>; S C Balawat <scb12345@gmail.com>; sanggyu LEE <sgleehong@gmail.com>; santhosh kumar <santhoshgu7@gmail.com>; SAQIB SHIRAZI <saqibshirazi83@hotmail.com>; sevak hiren <hirensevak80@gmail.com>; Shadab Alam Ansari <shadabansaria...@gmail.com>; shanmuga mari <85.ssmari@gmail.com>; snbagchi <snbagchi@aol.in>; Srinivas Engr <srinivas.gmsrini@gmail.com>; srinivasu <srinivasu.mech@gmail.com>; T. Mahendran <cbemahendar@yahoo.com>; U WYNN-NAING <u.wynn-naing@total.com>; vaibhav Joshi <vnjoshi.leo@gmail.com>; venkat ramana <venkatgps.ramana@gmail.com>; Vijay Katkar <katkar.vijay22@gmail.com>; vinit.deshpande <vinit.deshpande@akersolutions.com>; Vino Varghese <vinopvarghese@gmail.com>; Wu Hua <jointstars@yahoo.com>; yogeshkumar Kumbhar <kumbharyogeshv@gmail.com>; ZUL MAS <zulmas77@yahoo.com>
Sent: Wednesday, April 11, 2012 9:11 AM
Subject: Regarding Electrode Weaving

 

Respected Experts,


We generally mention in WPS/PQR weaving of Electrode should be three times the Electrode dia...I have query is Code restrict for this ,anywhere written in code aur it is on general experience...


Thanks & Regards
Mohit Aggarwal

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Any views or opinions expressed in this email and its attachments are those of the individual sender except where the sender specifically states them to be that of Lamprell.

This E-mail and any attachments are confidential and may also be legally privileged. If you have received this email and any attachments in error, you are on notice of its status. Please (a) notify the sender immediately by reply email; (b) destroy this email and any attachment, and (c) do not use, copy, store and/or disclose to any person this email and any attachments: to do so could be a breach of confidence. Thank you for your co operation. Please contact the Lamprell IT Helpdesk on ithelpdesk@lamprell.com if you need any assistance.

Holding company: Lamprell plc, incorporated in the Isle of Man, registration number 117101C, registered office at Fort Anne, Douglas, Isle of Man IM1 5PD

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...