[MW:14098] RE: 14088] Max allowable offset

The best approach to this is to make issue that the thickness differentials is evenly distributed all over the circumference on both the ID and OD. You can do this by checking fit-up alignment properly using the required alignment measuring tools.

 

Hope this is helpful.      

 

“Quality is the Bone, Be the Dog Always”

 

Boniface Obidike

QA/QC Engineer

Speciality Connectors & Pipesi

Mail: Boniface.Obidike@ge.com

Office: +234(1)4629400

Mobile: +2348163479738

Home: +2348039409934

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sevak hiren
Sent: Tuesday, April 10, 2012 6:38 PM
To: materials-welding@googlegroups.com
Subject: [MW:14088] Max allowable offset

 

Dear experts,  I have a question. For circumferencial joint joining two thicknesses for a pressure vessel  e.g. 8 mm and 10.5 mm what is maximum allowable offset ?  As per uw 33 it comes out to be 2 mm .my question is it can not be tapered transition as the thk difference is less than 3 mm as per uw 9.  Now if we match ID then the offset will be 2.5 mm and we can not taper the joints also.  Please suggest.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...