[MW:14154] PWHT OF P 91 ALLOY STEEL MATERIAL.

Dear All,
 
 We are going to do P91 piping fabrication,   as per client specification the stroage time after welding is limited to maximum 7 days for PWHT.  Is there any problem if it delays 10 days when  we are  following preheating procedure for welding as mentioned below:
 
 Preheat at 200 degree C.  Min. 300 degree C. Max.
 Inter pass temperature  250  to 300 degree C.
 Cooling 20  to 80 degree C. after wleding
 Post heating (extended heating) after cooling 300 degree C.   
 for four hours or 400 degree C. for three hours.
 
Thanks in advance for your response.\
 
Manoj.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...