[MW:14157] weld hard spots on castings

Dear Experts,

Can anybody  clarify me with literature.

We have typical problem like this:

We are making small cosmetic weld on castings - P1 materials ( WCC and LCC)
Process used is SMAW. we use welding electrode E 7018-1.
We use a preheat of 45-95 Deg C.Interpass being 300 deg C.PWHT is done @ 610 deg C.
We had already demonstrated PQR with the parameters like electrode,current, preheat, interpass,and PWHT, the same are being excercised in the production weld also.
Once after PWHT when we check hardness using portable (Equo-tip) hardness tester we find some welded spots shows high hardness which exceeds NACE  requirements (237 HB).
We are facing similar high hard spot on material ASTM A 487- 4C material also.

MANIVANNAN.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...