[MW:14128] Re: regarding- thickness range for LTCS piping material for WPS

what is your design code?
As per ASME it will be T-2T, however for piping (B31.3) this range can
be used if PTC's are provided for the thickness ranges as specified in
Table 323.3.1, else it will be T to T+6mm

Best regards

On Apr 19, 10:42 am, Darshan Maheshwari <darshan.maheshw...@yahoo.com>
wrote:
> Can any body suggest what thickness range is applied for qualifying a WPS (for thickness 7.11mm) for LTCS piping material. Please provide reference also.
>
> Regards,
>
> Darshan Maheshwari.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...