Wednesday, April 11, 2012

[MW:14094] IS 1030 steel castings

Dear all,
 
Can any one tell the equivalent EN grouping / ASTM number for IS 1030 280-520W 

Thanks & Regards,

Srikanth chavali,
Engineer-Welding Technology,
Thyssen Krupp Industries (India) Pvt. Ltd.,
Hyderabad.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/