Dear Friend,
You can used high heat input per meter with controlled cooling (slow cooling), by doing this u  can achieved your required standard hardness i.e 225 BHN: ( my experience says u can achieve below 225, which is good)

Best Regards
huzaifa

QA/QC Engineer
B.E/M.S in Materials Science

People Steel Mills Karachi
pakistan





 
Dear experts,
I have faced regarding hardness issue on ASTM A 335 GR P-11 material.
Pipe thickness is 7.5mm.  Without PWHT hardness is coming around 275
to 289 BHN  on weld zone & 250 260 BHN on HAZ zone & parent material
hardness is 197 to 204 BHN. Due to inside refractory material PWHT is
not possible.
My question is as per ASME B-31.3/ ASME SEC II PART A hardness value
of this material is 225 BHN ( MAX).  There is any specification for
weld zone / HAZ zone hardness value.
Can anybody give an idea to reduce the hardness without PWHT  if it is
not acceptable limit.
Thanx in advance.

Regards
Pradip

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...