Re: [MW:14127] suitables electrode used for cast iron

DEAR FRIEND,
IF YOU USED LOW HYDROGEN ELECTRODE FOR CAST FE 7& HIGH STRENGTH MATERIAL, THE WELD WILL CRACK OR MAY CRACK IN FUTURE
THE MOST SUITABLE ELECTRODE FOR THIS TYPE OF JOINTS IS ANY HIGH PERCENT NICKEL ELECTRODE.
FOR ANY QUERY U MAY CALL +923312041785
OR CONTACT ON engr.huzaifa@gmail.com

REGARDS
HUZAIFA
QA/QC ENGR
PEOPLE STEEL MILLS KHI


On Tue, Apr 17, 2012 at 2:39 PM, izzuddin mustafa <ezzudine@yahoo.com> wrote:
Hi experts,

I need your help. I prepared procedure to welding panama chock (cast iron material)  to high tensile strength plate (EH 36). what is the suitable eloctrode to used for smaw process? can i used the  ordinary low hidrogen eloctrode such as KOBE brand E 7018? or special elctrode? please advice me.

Thank you.

Ezzudine Must.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...